Joist spacing for composite decking is the centre-to-centre distance between the support beams under the boards — 400 mm (16 in) for residential decks and 300 mm (12 in) for commercial loads. Because composite decking flexes more than timber, spacing controls the "bounce" a buyer feels and the warranty a supplier honors.
Key Takeaways
- 400 mm (16 in) on centre is the residential standard in the US, UK and Europe; commercial decks carrying 5 kN/m² design loads step down to 300 mm (12 in), and some Australian brands publish up to 450 mm for specific residential profiles.
- 21–24 mm boards top out at 400 mm spans, while 25 mm+ boards are rated up to 500 mm — board thickness is a framing-cost lever.
- End gaps of 6–8 mm plus 3 mm side gaps absorb thermal movement; missing them is a main reason warranty claims get rejected.
- Plan for roughly 19 hidden fastener clips per square metre at 400 mm centres and 24 at 300 mm — one clip at every joist crossing, in 316 stainless for coastal sites.
Composite Decking Joist Spacing: Reference Tables by Application
The table below consolidates joist spacing figures from manufacturer installation guides (Deckorators, Millboard, Trex) and UK/European trade guidance (Howarth Timber, TradeFox).
| Application | Board layout | Joist spacing (centre-to-centre) | Design load |
|---|---|---|---|
| Residential deck, terrace, garden | Straight, 90° to joists | 400 mm (16 in) OC | 2.5 kN/m² |
| Commercial — pubs, restaurants, retail, boardwalks | Straight, 90° to joists | 300 mm (12 in) OC | 5 kN/m² |
| Diagonal 45° / chevron pattern (residential or commercial) | 45° to joists | 300 mm (12 in) OC | — |
| Diagonal 30° layout | 30° to joists | ~350 mm (14 in) OC — the same cut as 60° in Trex's chart convention | — |
| Flexible product lines (e.g., some Trex profiles) | Straight | 300–350 mm OC | per datasheet |
North American figures run on psf ratings instead of kN/m². The IRC/IBC floor for residential walking surfaces is 40 psf, but Trex's 1×6 lines are third-party tested (ASTM D7032) to 100 psf at 16 in OC — and 12 in OC lifts the same boards to 200 psf for commercial use. In metric terms that mirrors the 2.5 kN/m² / 5 kN/m² split above, and 2×6 (51 mm) Trex boards add another step: 24 in OC at 100 psf, 16 in at 200 psf.
Angled layouts have their own reduction rule, though brands measure the angle differently — some off the joist line, others off the perpendicular. Trex's published rule, measured off the joist: at 60° reduce the straight-run span by 2 in, at 45° reduce by 4 in (400 mm → 300 mm), and at 30° use half the listed span. A "30° diagonal" in the perpendicular convention is the same cut as Trex's 60° — which is why published 30° figures sit near 350 mm (14 in) while Trex's shallow-angle rule is far tighter. Chevron and picture-frame details, where boards change direction at seams, take the 45° figure.
Codes and market norms worth checking per destination:
- US: the 16 in grid clears both worlds at once — 40 psf residential by code, 100 psf tested for 1×6 boards, 200 psf at 12 in OC where commercial plans demand it.
- UK/Europe: 400 mm centres is common practice for domestic decks; 300 mm covers commercial and public use.
- Australia/NZ: brand norms run wider — Ekodeck publishes 450 mm maximum residential centres for its Classic and Flame Fighter profiles under AS/NZS 1170.1 domestic loads (1.5–2.0 kPa), stepping to 400 mm for commercial work, stairs and landings. Check the destination brand's datasheet rather than importing a foreign habit.
- Retrofit warning: existing timber frames at 24 in (600 mm) must be sistered down before composite goes on; Trex's guide voids the warranty on 24 in frames that were not re-spaced.
How composite spacing compares with what timber crews are used to:
| Framing habit | Timber (softwood) deck boards | Composite decking |
|---|---|---|
| Straight residential | 450 mm (18 in) centres, sometimes 24 in | 400 mm (16 in) max — most brands |
| Diagonal / picture frame | 400 mm | 300 mm (12 in) |
| Stair treads | case by case | down to 225 mm (9 in) for some Trex products |
Three rules sit behind these tables:
- Straight runs at 400 mm are the buying benchmark. When you quote a residential project, price the substructure at 400 mm centres. Most mid-range composite products are rated for it, and any product that is not will force extra joists into your costing.
- Commercial means 300 mm, no negotiation. Millboard's Lasta-Grip specification sheet publishes 5 kN/m² design loads for commercial decks versus 2.5 kN/m² residential — double the load means the span drops from 400 mm to 300 mm. Public-access projects (hotel terraces, waterfront boardwalks, school yards) always get the tighter figure.
- Diagonal and chevron layouts cost more than boards. At 45° the effective unsupported span between joists lengthens, so Deckorators, Howarth Timber and most North American brand guides (Trex, TimberTech/AZEK) all move to 300 mm (12 in) centres. Order the extra 10–15% board volume noted in the site notes below.
A fourth point for buyers: uneven spacing is worse than wide spacing. Composite decks fail early when joist centres drift between 350 mm and 450 mm across the same frame, because thermal movement concentrates at the widest bays and lifts boards or pops clips. Specify joist positions on your installation drawing, not "about 400 mm."

Composite Decking Joist Spacing vs. Board Thickness
Board thickness is the second half of the spacing equation. Thinner boards deflect more between supports, so their maximum span shrinks; thicker boards hold their line across wider joist bays, which saves framing timber and labour.
| Board thickness (typical export profiles) | Maximum joist span, straight layout | Notes |
|---|---|---|
| 21–24 mm hollow or solid core | 300–400 mm | Most 21 mm products are rated to 400 mm residential max; TradeFox guidance pushes composite under 25 mm down to 300 mm centres |
| 25–27 mm capped solid core | 400–500 mm | 25 mm is the volume thickness across the brands referenced in this guide; Eva-Last's 25.4 mm Pacific Pearl profile is rated for spans up to 500 mm |
| 30–33 mm heavy commercial | 500 mm standard; 600 mm only where the product datasheet expressly allows it [needs verification] | Used for boardwalks, heavy footfall, vehicle-edge applications |
Span economics work like this: at 400 mm centres a deck frame carries roughly 2.5 joist-metres per square metre of deck, at 300 mm it carries 3.3, and at 500 mm only 2. A 25 mm board with a published 500 mm rating therefore deletes about 20% of the joists, the joist tape and the blocking compared with the same deck framed at 400 mm — which is why premium 25 mm+ lines advertise span ratings, not just surface finishes.
What this means in a buying decision:
- If your market is residential DIY and contractor trade, order 25 mm boards and sell them with a 400 mm joist specification. That pairing matches most of the global composite decking market.
- If your client frames at 500 mm to save joist cost, you must supply 25 mm+ boards with a published 500 mm span rating — and the datasheet goes into the project file, because the warranty follows the datasheet.
- If the project is commercial, buy 30 mm+ boards AND frame at 300 mm. Thick boards do not license wider commercial spacing; the 5 kN/m² load class controls, not the board stiffness.
- Every board must bear on at least three joists — two full bays minimum — including the end bays. A board tail cut short of its third joist flexes at the edge forever.
- Some product lines publish tighter-than-normal figures, down to 300 mm for straight residential runs or 250 mm centres for very flexible thin profiles [needs verification]. Treat the board datasheet as the contract: it overrides every generic table on this page.
WPC Decking Board Size Reference for Importers
Factory catalogues and HS-code paperwork usually call the dimensions below "WPC decking board size" — the technical name for composite decking board dimensions. Knowing the standard sizes matters for two buying reasons: container yield and installer familiarity.
Widths
| Width | Where you see it |
|---|---|
| 135–138 mm | Slim-line profiles, often paired with 25 mm thickness |
| 140 mm | The most common export width; matches the 5½ in nominal lumber habit |
| 150 mm | Close second; preferred for wide-plank looks and 30 mm commercial boards |
| 160–200 mm | Wide fascia and feature boards, not primary deck surface |
Thicknesses
| Thickness | Typical use |
|---|---|
| 21 mm | Value lines, sheltered residential, high container yield |
| 25 mm | The volume thickness — most capping, most clip systems, most stock |
| 27 mm | Premium residential, wider span ratings |
| 30–33 mm | Commercial, boardwalk, heavy traffic |
Lengths
| Metric | Imperial | Container note |
|---|---|---|
| 2.2 m | 7 ft 3 in | Fits 15 pallets per 20 ft container when palletized |
| 2.9 m | 9 ft 6 in | Common European/UK module |
| 3.6 m | 11 ft 10 in | Long residential board, needs 40 ft container planning |
| 4.0 m | 13 ft 1 in | Popular in Australia/New Zealand |
| 4.88 m | 16 ft | North American 16 ft module; 20 ft container impossible, plan 40 ft |
| 5.4–5.8 m | 17 ft 9 in – 19 ft | Trex Transcend-style long boards; 40 ft container only |
Buyer checks on board size:
- Confirm the finished size vs. nominal size on the datasheet — a "25 mm" board may measure 24 mm after capping and sanding.
- Remember longer boards move more. Thermal expansion is proportional to length, so a 4.88 m board needs the same percentage gap as a 2.2 m board, but the absolute gap is larger. Long boards also raise freight cost per metre because 20 ft containers cannot take them.
- Ask the factory for the pallet and container yield table before committing to a length — changing 2.9 m to 3.6 m can drop a 20 ft container load by 15–20%.
- Match board size to your clip system. Most universal clips fit grooved 140–150 mm boards of 21–27 mm; 30 mm+ boards usually take the factory's own heavy clip.

Tongue and Groove Composite Decking: Profiles Explained
A deck with no visible fixings starts at the board edge. Tongue and groove composite decking interlocks — tongue on one edge, groove on the other — so fasteners hide inside the joint and the surface runs as one continuous field. In practice, the composite industry works with four edge/profile families:
| Profile | Edge detail | Fixing method |
|---|---|---|
| Tongue and groove (T&G) | Full interlocking tongue and milled groove | Boards seat into one another; clips or T&G-specific brackets at joists |
| Grooved edge (double side-groove) | Milled slot on both edges | Hidden T-clips slide into the groove, screwed to the joist; the next board hides the clip |
| Square/solid edge | Plain rectangular edge | Face-fixed with color-matched screws and plugs, or grooved on site with a router |
| Hollow core (open ends) | Internal chambers, scalloped back | Same clip fixing, but cut board ends must take end caps |
Profile checks for buyers:
- Grooved edge + T-clip is the volume system. One clip at every joist crossing holds the board; the next board's groove covers the clip, so the deck surface shows no screws.
- Tongue and groove boards need the factory's matching bracket. Generic T-clips designed for side grooves do not grip a full T&G joint reliably — order clips and boards from the same factory.
- Solid square-edge boards are the face-fixing option. Where a client wants a screw-down look, supply composite decking screws matched to the board colour (suppliers run pre-matched screw and plug kits by board shade) and specify pre-drilled holes to prevent mushrooming.
- Hollow boards show open chambers when cut. Budget end caps, picture-frame borders or full-perimeter fascias into every hollow-core project, and check that the factory's end caps match the cut profile exactly.
How to Install Composite Decking: A Step-by-Step Checklist
This is the checklist version of composite decking installation, ordered the way a site team actually works. The first half covers the substructure; the second half covers the boards.
Substructure checklist — complete before any board is cut
- [ ] Joists levelled and set at the specified centres — 400 mm residential, 300 mm commercial or diagonal.
- [ ] Frame level within 3 mm (1/8 in) over 3 m (10 ft) — composite telegraphs every hump and crown through the surface.
- [ ] Frame laid with a 1% drainage slope (10 mm drop per metre) away from the building.
- [ ] 100–150 mm clear ventilation gap between ground and joist underside (US contractor practice runs up to 6 in under the frame).
- [ ] Joist tape (butyl) applied to the top face of every timber joist before the first board.
- [ ] Framing material checked: pressure-treated timber at 0.25 lbs/cu ft retention minimum, or galvanised/steel/aluminium framing for roof terraces and wet sites.
- [ ] Blocking fitted between joists every 1.2–1.8 m to stop twisting.
- [ ] Sister (double) joists fitted wherever two board ends will meet at a butt joint.
- [ ] Extra joists or solid bridging added under heavy point loads (BBQ, spa, fire pit).
- [ ] Boards acclimatised flat on site for 24 hours before cutting.
- [ ] Weather check: installation temperature above 0 °C — most factories void cold-fit claims.
Board installation checklist — from starter row to final trim
- Set the first board along a chalked line, groove side facing the field, and fix the outer edge with starter clips or countersunk face screws at every joist.
- Fit a clip at every joist crossing — for 140 mm boards that is about 19 clips per square metre at 400 mm centres and 24 at 300 mm (7 board rows per metre of width against 2.5 or 3.3 joist-metres).
- Drive clip screws halfway and leave them; sliding the next boards seats everything, then you return and tighten. The screw head rests on the clip — never sunk into it.
- Slide the next board into the clips at a slight angle, tap with a rubber mallet until the gap is even, and repeat. One board end never shares a single clip with the next — butt joints get one clip per board on the sister joist.
- Stagger butt joints so adjacent row ends land at least two joist bays apart; a line of joints down one bay concentrates movement in one spot.
- Check square every ten boards and correct drift while the clips are still half-tight.
- Trim the last board to width and fix its outer edge with starter clips or face screws and plugs.
- Set the expansion gaps as you go, not afterwards: 6 mm at board ends (8 mm uncapped), 3 mm on sides, 10–20 mm off walls and posts.
- Cap the cut ends of hollow boards, then sweep the deck — metal shavings and grit left on the surface stain capped boards within weeks.
Tools worth writing into your installer's kit list: circular saw with fine-tooth blade, drill driver with adjustable clutch (no impact driver on clips), rubber mallet, chalk line, spacers, and a depth-setting bit for face fixing.

Seven Installation Mistakes That Void Composite Decking Warranties
Brand warranties are conditional documents: "if the manufacturer's instructions are not followed, any warranties given are voided" is standard wording. In warranty claims our export team has handled, these seven mistakes recur in nearly every file — hand this list to installers before the first board arrives.
- Skipping the datasheet. Trex, TimberTech and Fiberon use different formulations, different expansion rates and different clip systems. A timber crew's "standard practice" does not transfer.
- Mixing fastener brands. TimberTech's written rule is that clips made for one product line (AZEK) cannot be used on another (EDGE). Clip geometry sets the gap; the wrong clip sets the wrong gap.
- Building the frame like a timber deck. Timber boards ride 450 mm or even 24 in centres; composite tops out at 400 mm straight and 300 mm diagonal. Old 24 in timber framing must be sistered down to the composite figure.
- Setting gaps by eye. One 30 °C afternoon changes a board's length by millimetres — every gap on the deck is a calculation, not a habit.
- Starving the underside of air. Frames sitting close over damp ground trap moisture against the board underside; the boards grey and cup, and the claim dies on "inadequate ventilation."
- Overdriving clips. An impact driver on a clip cracks the plastic or the board groove. Torque control only, and the screw head rests on the clip.
- Cutting after the wrong acclimatisation. Boards stored upright in the sun bow before installation; flat storage for 24 hours on site is part of the installation spec.
The expensive consequence of any of these is not the material — it is the redo. Installers report tearing out buckled sections two or three years after handover, and the debate over who pays falls on whoever skipped the checklist.
Composite Decking Expansion Gap Table
Composite decking is roughly half wood fibre, half polymer. It expands in heat and contracts in cold — thermal expansion coefficients run around 33–36 × 10⁻⁶/K for capped boards and 44–46 × 10⁻⁶/K for uncapped, which is why gap discipline decides whether a deck stays flat for ten years or lifts in its first summer.
| Gap location | Capped board | Uncapped board |
|---|---|---|
| Board ends (butt joints) | 6 mm | 8 mm |
| Board sides (between boards) | 3 mm | 3 mm |
| Against walls, posts, fixed structures | 10–20 mm | 10–20 mm |
| Diagonal/angled cut joints | 6 mm | 8 mm |
Temperature-adjusted end gaps from the two most-cited fitting tables:
| Air temperature at installation | Ultradecking | NeoTimber |
|---|---|---|
| Above 25 °C (boards already expanded) | 4 mm | 1 mm |
| 4–25 °C | 6 mm | 3 mm |
| 1–10 °C | 8 mm | — |
| Below 1–4 °C (boards contracted) | 10 mm | 6 mm |
The two brands' tables diverge because their boards use different polymer blends and capping — use whichever belongs to the boards you actually bought, not a blend of both. Trex's imperial equivalents follow the same logic: 1/8 in (3 mm) end gap above 40 °F, 3/16 in (5 mm) below 40 °F, side gaps of at least 3/16 in, and 1/4–1/2 in (6–12 mm) where boards meet walls and fixed structures.
Practical gap rules for site teams:
- Hot-day fitting: boards are near maximum length, so fit ends tight or at 1–4 mm. Ekodeck's guidance: a full 6 mm gap set on a 30 °C afternoon opens to about 10 mm after the boards cool — that gap never closes.
- Cold-day fitting: set the large end of the range; boards will grow into it when the sun returns.
- Dark boards expand more than light ones — a charcoal board in direct sun runs hotter than an oak shade and needs its gaps respected, not guessed.
- Wet, wooded or enclosed sites: increase board-to-board gapping to 10 mm (3/8 in) per Trex's guidance for high-moisture locations.
- Perimeter gaps get covered, not closed. A 15 mm wall gap hides under an L-corner or fascia profile; a 2 mm wall gap buckles the frame.
Composite Decking Screws and Fastener Selection
Composite decking screws are the visible-face option; hidden clips are the invisible option. The decision tree below matches fastener to environment and profile.
| Situation | Fastener to specify |
|---|---|
| Coastal, marine, salt-spray sites | 316 (A4) stainless steel screws and clips — the marine grade; 304 (A2) tarnishes under constant salt exposure |
| General outdoor, inland | 304 (A2) stainless or epoxy/nano-coated steel screws |
| Face-fixed boards, any site | Pre-drilled holes + color-matched composite decking screws (reverse-thread or plug systems prevent mushrooming) |
| Grooved boards, standard runs | T-clips (metal, with integrated gap tab) at every joist |
| First/last rows and edge boards | Starter clips or face screws — standard T-clips cannot reach the outer edge |
| Boards on expansion-sensitive frames | CEC/expansion clips that hold the board down while letting it slide |
| Perimeter, picture frames, stairs | Plug systems (screw through the face, tap the matching plug flush) |
Clip types you will meet in catalogues, with what each one is for:
- T-clips — the workhorse; the upright fin seats in the board's side groove, the base screws to the joist, and the tab sets the gap.
- Starter clips — one-sided version for the first and last board.
- Wedge clips — polymer wedges with stainless reinforcement, hammered in by hand.
- CEC (control expansion/contraction) clips — let the board slide lengthwise on high-movement frames.
- Collated strip clips — 16 clips pre-assembled on a strip for one-pass pneumatic or driver installation on large commercial decks.
Coverage arithmetic for ordering: at 16 in OC, Starborn's collated Clip&Rip runs about 175 clips per 100 sq ft (≈19 per m²) and 210 at 12 in OC (≈23 per m²); KOORF's kits quote 200 clips for roughly 100 sq ft at 16 in OC or 80 sq ft at 12 in OC. The quick way to estimate: a 140 mm board puts about 7 rows into a metre of deck width, and 400 mm centres put 2.5 joist-metres under each metre of deck — about 18 clips/m² — so estimate 18–24 clips per square metre across the 400–300 mm range and let butt joints and cut rows push it up.
Clip failure modes to eliminate:
- One clip per joist per board — skipping a joist to save clips is the single fastest way to a bouncy deck.
- Half-tighten on the first pass, final-tighten after the field is laid; a clip screw driven home early locks boards against the gap tabs.
- Torque control only — no impact drivers on clips (mistake #6 above).
- Never mix clip brands on one deck; gap widths differ between systems and the rows will read crooked.
- Face fixing follows the brand's plug system: pre-drill the pilot (3/16 in for Cortex-style systems), drive with the setting tool, tap the plug flush with a smooth-faced hammer.
Composite Decking Installation: Site Notes for Contractors
Short notes that keep an installation out of trouble — pass these to whoever frames and fits:
- Board overhang at edges: 50 mm maximum. Most brand guides run 25–50 mm (Trex caps perpendicular overhang at 3/4 in / 19 mm; Ekodeck at 20 mm); anything longer acts as a lever, so trim rather than overhang.
- Sister every butt joint. Two board ends meeting mid-bay on a single joist means each end hangs off half the bearing. Double joists with one clip per board is the only accepted detail.
- Size joists from the supplier's table. UK merchants stock decking joists from 47 × 150 mm upward, with 47 × 175 mm and 47 × 245 mm sections for longer bays [needs verification]; steel and aluminium systems take their own charts.
- 1% slope minimum on the finished deck, and the slope lives in the frame — not in shims under the boards.
- Ventilation below the deck is part of the warranty. 100–150 mm clearance under joists; Trex's manual says to leave openings under the deck or increase gapping to 10 mm where airflow is restricted. Do not lay composite directly over solid surfaces (concrete roofs, terraces) without a sleeper system that breathes.
- Boards go down at 0 °C and above. Below freezing the boards are stiff and brittle; cold-weather installation is a listed exclusion on several brand warranties.
- Diagonal orders: add 10–15% material for offcuts, and confirm the 300 mm joist grid before the frame goes in — retrofitting means sistering every bay.
- Align embossed grain in one direction and cut board ends before fitting; mixed grain directions read as a colour mismatch even in the same batch.
- Route grooves carefully on square-edge boards. A sloppy site-cut groove defeats the clip's grip; factories will groove boards in production if you order it.
Export Packaging and Delivery Checklist for Composite Decking
A standard export pack for composite decking includes, in order: protective film on the board face, corner guards on the bundle ends, shrink-wrap bundling, palletisation and container moisture control.
- [ ] Protective film (PE) applied to the face of every board before bundling — it peels off after installation and stops scuffing in transit.
- [ ] Corner guards on both ends of every bundle — board corners chip first in handling, and chipped corners are the top transit damage claim on WPC decking.
- [ ] Shrink-wrap bundling, standard 3 boards per bundle.
- [ ] ~56 bundles (168 boards, roughly 55 m²) per pallet; 2.2 m boards palletize to ~15 pallets per 20 ft container.
- [ ] Nylon fabric cover over each pallet with PE straps; soft cushioning between pallets in the container.
- [ ] Desiccant bags inside the container — "container rain" condensation stains uncapped boards permanently.
- [ ] Clips, screws and end caps packed separately in cartons, counted against the board order — a missing accessory box stops a site for a week.
- [ ] Photographed loading report with pallet counts before sealing — the buyer's claim file if anything shifts in transit.
Delivery inspection, buyer side — check on arrival before signing the carrier's papers:
- [ ] Film intact on sampled boards; film-stripped boards are re-wrapped only on request.
- [ ] Corner guards present and unbent on both ends of every bundle.
- [ ] No moisture staining inside the shrink wrap (desiccant failure shows up fast).
- [ ] Bundle count and carton count match the packing list exactly.
Pre-Order Checklist: What to Lock Down Before You Buy
- [ ] Board profile, width, thickness and length confirmed against our catalogue — see the full composite decking range for standard lines and custom options.
- [ ] Joist spacing spec written into the order: 400 mm residential, 300 mm commercial or diagonal.
- [ ] Fastener package matched to site environment — 316 stainless for coastal projects.
- [ ] Factory span and deflection test report (ASTM D7032 or EN equivalent) on file before the order ships.
- [ ] Landed cost per square metre calculated with container yield — see current composite decking price benchmarks for FOB and freight ranges.
- [ ] Maintenance commitment agreed with the end client — see how to clean composite decking for the aftercare sheet to hand over.
- [ ] Packing standard (film + corner guards + desiccant) written into the purchase order.
FAQ
Q: What joist spacing should I use for composite decking?
Use 400 mm (16 in) on centre for residential straight runs and 300 mm (12 in) for commercial decks or any 45° diagonal/chevron layout; Australian brands such as Ekodeck publish up to 450 mm for some residential profiles, so check the datasheet for the destination market.
Q: Can 21 mm composite decking span 500 mm joists?
No — 21–24 mm boards are rated to 400 mm maximum and many product lines push them to 300 mm; 500 mm spans need 25 mm+ boards with a published span rating on the datasheet.
Q: What screws should I use for composite decking near the coast?
Specify 316 (A4) marine-grade stainless steel for screws and clips; 304 (A2) stainless is acceptable inland but will tarnish under constant salt spray.
Q: How much expansion gap do composite decking boards need?
Leave 6 mm at board ends for capped boards (8 mm uncapped), 3 mm on side edges, and 10–20 mm against walls — and widen end gaps in cold weather since boards contract and expand again with heat.
Sourcing WPC Decking?
Send your specification, quantity, destination and timeline. Fides routes the request to relevant WPC decking companies.